O T H M A N
S H A R I D A H
C O N T R A C T I N G
Introduction
  • Non-metallic GRP/RTR/FRP/RTRP/GRE/GRV pipes.

  • Metallic high temperature lines up to 250ᵒC

  • When pipes develop defects such as
  • Dents and chips

  • Wall thickness loss

  • Delamination

  • Burned particles

  • Damage to fiber backing

  • Resin rich layer surface totally dried out

Features and characteristics

  • Superior alternative to clamps.

  • All pipe sizes.

  • Straight length, elbows, tees.

  • No hot works./No welding.

  • Engineered solution.

  • Supplied as a complete kit.

  • Compatible with carbon steel

  • CFW (PAN-Polyacrylnitrile)

  • High corrosion resistance.

  • Chemically resistant.

  • Able stand high temperatures.

  • High strength.

  • Long service life.

  • No VOCs.

  • DIAMONDWRAP 100% solids .

  • Fast curing.

  • Extensively tested in field.

  • systems for chemical resistance.

  • 00

    %

    Success Rate

  • 00

    +

    Happy Clients

For the above defects below are 3 possible solutions.
  • Replace the defected pipe and have a costly shutdown.

  • Repair the defected pipe on site again with a shutdown (depends on method and line)

  • Repair without shutdown with easy to install non-metallic composite materials.


In consideration with the severity of the defect OSC will design the proposal based on 100% wall loss of the pipe by taking a safety factor into consideration.


All repairs are made in accordance with ASME PPC-2 2015 (Article 4)